Heat water to 75 C. Add hydroxyethyl cellulose with rapid agitation. Mix until fully dissolved and hydrated. Cool to 40 C. Add "merquat" 550 and Quaternium with stirring. Dissolve perfume in Octoxynol-9 and add. Continue mixing to 25 C. pH---4.8 Visc.---200 cps @ 25 C