Disperse "Carbopol" in water. Weigh # 1-7 and heat to 80-90 C with slow agitation. Add remaining ingredients, except triethanolamine, to the "Carbopol"/water dispersion and heat to 80-90 C. Add the aqueous phase to the wax phase and shear in homomixer for 5 min. Add triethanolamine and continue to shear while cooling to 40-50 C. Add perfume, deaerate, and package.