Disperse the "Carbopol" resin in water and glycerin, blend with vigorous stirring until uniform. Add the "laponite" and methyl paraben and stir until uniform. Combine the oil phase ingredients and heat to 75 C. Heat the dispersion of "Carbopol" resin to 75 C and add oil phase with high speed agitation until uniform emulsion is formed. Add the triethanolamine and continue stirring while cooling and add the "Dowicil" at 50 C and perfume at 40 C. Cool to 25 C and package.