Propylene glycol/10 Mix "Emcol" 249-3K, propylene glycol, sodium stearate and "Emcol" CDA and heat to 170'F. with mild agitation to form a homogeneous slurry. Add water and mix until homogeneous and clear. Discontinue heating, add perfume and mix until clear. Pour hot into molds or containers. The perfume level can be varied from 0 to 20 per cent with a corresponding adjustment of the level of "Emcol" 249-3K. The melting point of this stick can be changed by varying the ratio of propylene glycol and sodium stearate. An increase of propylene glycol with a corresponding decrease of sodium stearate results in a softer stick. FORMULA No.2 (Frosted Gleamer Mineral oil, 70 Visc./11.00 Perfume/1.00 "Tenox" 2/0.10 25% Solution in Castor Oil of D & C red no. 9 Ba Lake/11.00 Titanium Coated Mica/5.00 Water/3 Sodium stearate/8 Perfume/5 "Emcol" 249-3K/69 Ozokerite, 190'F M.P./17.50 Isopropyl lanolate/48.00
配制方法:
Heat to 90'C & mix; cool to 65'C; pour into molds; chill.