Recovery of Zinc from Dross (U.S. Patent 2,701,194)
配方组成:
Sodium Chloride/21 Barium Chloride/31 Fuse and ad Calcium Fluoride/3 Calcium Chloride/48
配制方法:
This flux melts at 850'F and can be heated to 1300'F without fuming. From 10 to 20% of this flux is stirred into the dross and rabbled until the oxides separate from the metal.