帮助中心
配方类型:
METALS
配方说明:
To Color Galvanized Iron (Japanese Patent 6610) (1959)
配方组成:
Cyanine Green/1.5
Diallylmaleate Semipolymer/15
Benzoyl Peroxide/1
Aluminum Powder/25
Diallylphthalate Semipolymer/60
配制方法:
Apply this mixture to metal, heat to 100'C for two minutes at 200'C for 15 minutes and cool.