China Wood Oil/25 Mineral Spirits/100 "Neville" LX-685, 135/75
配制方法:
The resin and oil are cooked at 500'F until a sample droplet remains clear at room temperature. The batch is then cooled and thinned with an equal amount of mineral spirits or to any desired range of viscosity. The addition of a trace of manganese naphthenate is suggested to speed the drying time.