Water/25 Thin amide by heating (perhaps add a little alcohol also) and spray a few percent onto the phosphates and other builders while tumbling. The powdered alkylaryl sulfonate is added last and mixed in briefly. Formula No.3 (Lotion Type "Nacconol" NR or "Santomerse" 1/25 Sodium Tripolyphosphate/30 "Ninol" AA62/3 "Stepanol" B-129/55 "Stepanate" X/10 "Ninol" OA/6 Urea/4 Sodium Sesquicarbonate/42
配制方法:
All the ingredients are stirred together except for the "Ninol" OA which is added last; the pH should be adjusted to 7.0 for best stability of the opacifier. In this formulation, the "Ninol" OA is an opacifying alkylolamide, and the "Stepanate" X and urea act as stabilizers.