Zinc Oxide/80 g Dioctyl Sodium Sulfosuccinate/0.65 g Glycerol/30 cc Calamine/80 g Water/960 cc CMC-7MP/20 g total Volume, about/1000 cc
配制方法:
Dissolve the cellulose gum in 600 cc of water with vigorous stirring; then, with slow stirring, add 295 cc of water. Add next the dioctyl sodium sulfosuccinate previously dissolved in 65 cc of water. Rub the calamine and zinc oxide to a smooth paste with the glycerol and about 40 cc of the prepared suspension base. To this add the remainder of the base in small portions, mixing after each addition, or, add slowly with continuous mixing.