Triethanolamine/4.30 % by wt Perfume Truodor #53/0.50 % by wt Water/76.60 % by wt Water Phas Hexadecyl Alcohol/2.0 % by wt b: Stearic Acid/4.75 % by wt Stearic Acid T.P./9.0 % by wt Coconut Fatty Acids/1.5 % by wt Glycerol/10.50 % by wt Triethanolamine/5.0 % by wt Coconut Fatty Acid/1.60 % by wt Water/82.5 or 100.0 % by wt Concentrate/93.0 % by wt Propellents 12:114 (57/43)*/7.0 % by wt a: "Veegum"/1.50 % by wt or Concentrate/96.0 % by wt Concentrate/93 Isobutane: Propane (70/30)/4.0 % by wt *U.S. Pat. 2,655,480 Propellent 12/114 60/40/7 "Vancide BN"/0.25 % by wt
配制方法:
Oil and water phases are heated separately to 75'C. The water phase is added to the oil phase with careful agitation to prevent entrainment of air. When the emulsion is well formed, the mixture is allowed to cool to room temperature with stirring. Perfume oil, as desired, may be added at 35'C. The propellent blend is added by pressure filling.