Prepare A by dispersing the "Carbopol" resin in water then add the remaining reagents in order listed. Heat to 80'C. Prepare B; heat to 80'C until completely dissolved. Add A slowly to B with good agitation (maintain 80'C). Add C to blend of A and B and cool to 40'C. Add D and mix until cool.