Methyl Paraben/0.25 Prepare B by dispersing the "Carbopol" in the water using moderate to high-shear agitation. Add the rest of the ingredients using moderate-shear mixing. Heat mixture to 75'C. Prepare A and heat to 75'C. Add A to B, mix to uniformity, and cool. FORMULA No. Sorbic Acid/0.2 "Nodorlan"/1.0 Lanolin/3.0 Mineral Oil (NF)/6.0 "Carbopol" 941 Resin/0.2 Water, Preservatives, Perfume, and Dye/71.6 Propyl Paraben/0.1 "Arlacel" 80/2.6 B: Water/54.4 A: "585 Cosmetic Liquid"/26.0 Dehyquart C/0.2 Propylene Glycol/10.0 "Standamul" G-16/10.0 Pectin (NF)/3.0 "Tween" 80/5.5 Glycerin/6.0