"Amerlate P"/1.0 "Ucon" 50HB660/5.0 Dissolve the "Tergitol" Surfactant 15-S-12 and preservative in the water. Add the "Polymer JR" while stirring, and continue mixing until the resin is dissolved. Introduce the alcohol into the formula. Finally, add perfume as desired. The use of hot water (60'C) will increase the rate of solution for Polymer JR. FORMULA No.3 (Clear Hair Setting Gel "Polymer JR"-400/1.00 "Tergitol" Nonionic Surfactant 15-S-12/0.05 Triethylene Glycol/0.05 Methyl p-Hydroxybenzoate/0.05 SD-40 Alcohol (anhydrous)/25.00 Deionized Water, Perfume/73.85 Polyoxyl 40 Monostearate (USP)/3.0 Mineral Oil (330 visc)/15.0 "Amerchol L-101"/5.0 A: "Uvinul" D-50/0.1 SD 40 Alcohol/15.0 "Carbopol" 940 Resin/0.4 Distilled Water/29.3 "Carbopol" 934 Resin/0.5 Perfume/q.s. B: "Solan"/2.5 "Sequesterene" Na4/0.1 Distilled Water/40.1 "Polyox" WSRN 3000/0.4 PVP K30/1.5 Glycerin/5.0
配制方法:
Disperse "Carbopol" 940 in the water shown in A. Dissolve the "Uvinul" and perfume in the alcohol of A. When the slurry containing "Carbopol" 940 is completely uniform, add the alcohol solution to complete A. Warm the water in B and dissolve the "Solan," then the "Sequesterene," "Polyox" and PVP in that order. Add the glycerin. Combine solutions A and B, then when uniform add the "Ucon" 50 HB660. Complete the gel by neutralizing with the amine. For ease of handling, some of the water from B may be used to make a more dilute amine solution.