Paraffin Wax (156'F, 68.8'C)/30.0 Toning Iron Blue/3.0 Methyl violet Base/0.1 Mineral Oil (100 SUS)/29.9 "Petrolite" WB-5/15.0 Furnace Black/22.0
配制方法:
Charge waxes and dyes in a steel ball mill at 200 215'F (93.3-101.6'C). Mill until dyes are in solution (15-30 min). The balance of the materials are added to the ball mill and milled for 2.5 h.