Preservative/q..s Place surfactant, alcohol, water and amide into suitable container. Warm to 80'C, mix gently until the surfactant has dissolved and the mixture is homogeneous. Add preservative and transfer to suitable containers. Product sets up into a clear, ringing gel when cooled to room temperature. FORMULA No. Other Isomers/.70 "MGK" 326/.99 "Tetronic" 1508/14 Isopropyl Alcohol/12 N,N-Diethyl-m-Toluamide/10 Water/64 Preservative/q.s. "MGK" 264/3.96 Deodorized Kerosene/80.21 N,N-Diethyl-m-Toluamide/13.15 "Polawax"/3.0 N,N-Diethyl-m-Toluamide/15.0 Ethanol SDA-40 (95%)/39.6 Water/32.4 "Poloxamer" 407 or Poloxamine 1508/14 Propellant 12/114 (40:60)/10.0 Isopropyl Alcohol/12 N,N-Diethyl-m-Toluamide/10 "MGK" 11/.99 Water/64