Triethanolamine/0.6 Heat both phases to 70'C. Add the water slowly to the oil phase with high speed stirring, allowing time for each addition to incorporate. When all in, cool with agitation to just above melting point and fill off. A homogenizer may be used to improve stability. FORMULA No. Petrolatum/5.0 Allantoin/0.25-0.5 Water/q.s.to 100 Coal Tar/2.0 Paraffin Wax 140/12.0 Allantoin/0.25-0.5 "Super Hartolan" Lanolin/4.0 Stearic Acid (triple pressed)/16.0 "Novol"/6.0 Water/q.s.to 100 Lanolin/2.0 Mineral Oil/30.0 Coal Tar/2.0
配制方法:
Heat both phases to 75-80'C add water to oils with high speed stirring. Cool to 40 with stirring and fill off.