Ceteareth-5/5 Add water, "Tetronic" polyol, propylene glycol, glyceryl monostearate, Ceteareth-5 and lanolin to mixing vessel. Warm gently to 60'C and mix in perfume and preservative. Transfer to containers. Product sets up into a viscous cream at room temperature. FORMULA No. "Pluronic" L-35/2.00 Perfume/10.00 Glyceryl Monostearate/10 Perfume/4 Water/61 Preservative/q.s. "Lexgard" M/0.15 "Pluronic" 17R8/16 Propylene Glycol/6 B: "Lexemul" 561/21.00 Glyceryl Monostearate/10 Lanolin/2 Stearic Acid/3 Perfume Oil/4 Water/59 Preservative/q.s. "Lexate" TA/10.00 "Lexgard" P/0.05 "Tetronic" 1504/2 A: Water/51.80 Propylene Glycol/6 Cetyl Alcohol/5.00 Lanolin/2
配制方法:
Add water, "Pluronic" polyol, propylene glycol, glyceryl stearate, stearic acid and lanolin to container. Warm gently to 60'C and mix well with a minimum of aeration, until mixture is homogeneous. Allow to cool to 45'C, add perfume oil and preservative, and mix well. transfer to containers and allow to cool to room temperature at which it sets up into a stiff gelatinous cream.