Place cold water (5-10'C) in container and add "Pluronic" F-127 polyol slowly with good agitation. Mix until all F-127 is dissolved, maintaining temperature at 10'C. Add depilatory ingredients, mix until homogeneous, and quickly transfer to containers. The product sets up into A ringing gel when it warms up to room temperature.