Water/5.0 "Geopon" GA-1/10.0 Propylene Glycol/2.5 Active Constituent/82.5
配制方法:
Blend the active constituent and "Geopon" GA-1 in a ribbon blender or similar peice of mixing equipment. Aspirate the water and propylene glycol into the blender and mix until uniform wetting is assured. Extrude through a pellet mill or extruder.