Tetrasodium Pyrophosphate/0.3 Water/100.0 Formula No.2 (White "Nopcosant" L/0.7 Red Iron Oxide/100.0 Titanium Dioxide Slurry/15.0 Calcium Carbonate Slurry/55.0
配制方法:
combine ingredients under agitation. If a finer dispersion is desired, the compound can be dispersed to a very fine consistency by ball milling or by grinding on a stone disc mill.