Add the "Veegum" to about 30 parts water, agitating continually until smooth. Add the zinc stearate with agitation. Add the cocoyl sarcosine to the paste. Premix D, add to A, B, and C and work into a smooth paste (add more water if necessary to get a paste). Pack into stick mold and allow to dry. Note: The final pH should be about 5.0.