配方类型:
RUBBER, RESINS, PLASTICS AND WAXES
配方说明:
Cation-Exchange Resin (Indian Patnet 47,468)
配方组成:
Formaldehyde/110 cc.
Naphthalene/52 g.
Sulfuric Acid (66'Be.)/33 cc.
配制方法:
Heat the naphthalene to 120'C. and add the acid, with stirring.
Then heat at 140 to 150'C. for 5 to 6 hours. Cool to 90'C. and add the formaldehyde, with good stirring, until a hard black resin results. Wash with water and regenerate with 5% hydrochloric acid.