帮助中心
配方类型:
MISCELLANEOUS
配方说明:
Atrazine Flowable Suspension
配方组成:
Propylene Glycol/7.50
Atrazine (98% tech.)/46.00
"Kelzan"/0.05
"Darvan" No.1/2.00
"AL" 1526/2.50
Water/41.35
Defoamer L-768/0.10
"Veegum"/0.40
Paraformaldehyde/0.10
配制方法:
This formulation has been prepared in 2 kg batches in a 1.3 gal ball mill half filled with 1.25 in . "Burundum" cylinders.
Add all ingredients, except "Kelzan," to the mill in the order listed.
The wetting agent is preferably first dispersed in the glycol. Mix until the atrazine needles are in the 1-5 \um range with at least 90% <= 5 \um. When using the ball mill, approximately 5 h of grinding time is required to achieve the desired particle size. Add the "Kelzan" and mill for 30 min or until completely dissolved.