帮助中心
配方类型:
MISCELLANEOUS
配方说明:
Windshield Deicer
配方组成:
B: Water/50.0-100.0
Formula No.11 (Polybutene-Nonionic
Deionized Water/to 100.000
Polybutene/100.0
Ethylene Glycol/5.000
Oleic Acid/3.5
Triethanolamine/1.7
Water/67.0
Sodium Sulfate/0.085
Polybutene/100.0
"Triton" X-400/20.0
Water/67.3
A: Mineral Oil/90.0
Isopropyl Alcohol/10.000
Polybutene/100
Alkyl Phenoxy Polyethoxy Ethanol/4
"Siponic" 218/-
"Arosurf" 90E20/10.0
Water/29
"Laponite" RD/3.000
"Carbopol" 940/0.5-2.0
Polybutene/100
Alkyl Phenoxy Polyethoxy Ethanol/-
"Siponic" 218/5
Water/67
配制方法:
Mix polybutene with emulsifier in a high-speed, shear mixer such as a cowles Dissolver. Add water slowly until inversion occurs. Add remaining water more rapidly. Preheating both the polymer mixture and the water facilitates emulsification. With the higher viscosity polymers (>175 cs @ 99'C), temperatures of 65-90'C may be necessary.