Weigh and add the deionized water into a container and begin stirring and heating. Stir by means of a variable speed agitator equipped with a propeller-type stirrer. Slowly sprinkle in the magnesium aluminum silicate and bring temperature of the blend to 70-73'C. When all of the magnesium aluminum silicate has been added, modify the stirring process so that a variable speed agitator equipped with a stirrer for efficient blending is used. Caution should be exercised so that air is not incorporated into the product during mixing. Add Part B in order while mixing continuously. Continue mixing and cool to 40-43'C and add Part C. Package product into suitable containers at 25-30'C.