Grind iron oxide pigments in glycerol. Prepare 2% solution of sodium carboxymethylcellulose in water, stirring until uniform. Stir Part B ingredients together until smooth, heat to 90'C. While heating to 90'C, mix Part A ingredients until uniform; stir Part B into Part A. Cool to 40'C. Disperse pearl pigment. Add perfume with stirring.