配方类型:
METAL TREATMENTS
配方说明:
配方组成:
phosphoric acid/6
citric acid/15
water/1000
glucose/20
titanium potassium oxalate/50
配制方法:
anodizing is performed with 110 V ac at 75C and 5-6 A/dm^2.