perfume and preservative/q.s. B) "carbopol" 934 resin/0.5 "amerlate" P/1.0 water/60.0 triethanolamine/0.5 polyethylene glycol 1540 monostearate/3.0 A) "amerchol" L-101/5.0 alcohol/30.0
配制方法:
add the "carbopol" 934 resin slowly to the water at room temperature with rapid nagitation. mix thoroughly until a thin, cloudy dispersion is obatained. heat the solution containing "carbopol" resin and the oil phase separately to 75 C. add the solution with "carbopol" resin to part A and stir 5 min to emulsify. add the triethanolamine. cool with stirring to 38 C. add the alcohol and perfume and continue cooling to 30 C. NOTE: the "carbopol" 934 resin content may be adjusted to achiene varying conistencies.