potassium hydroxide/1.0 sorbitol (70% w/w)/10.0 water/4.0 A) stearic acid (triple pressed)/4.2 D) potassium sulfite/9.0 water/10.0 "arlatone" T/2.0 perfume/q.s. B) water/55.0 stripped coconut fatty acid/1.8 self-heating C) triethanolamine/3.0
配制方法:
heat part A ro 80 C. add part B and reheat to 80 C. add part C slowly, with agitation. mix for 30 min, maintaining temperature at 80 C. cool slowly while agitating slowly. add part D at 35 C. use a dual dispensing valve with 30 ml of 11% hydrogen peroxide in the plastic bag. fill: concentrate/96.0 propellant A-46/4.0