water/up to 100.0 glycerin/0.5 triethanolamine/to adjust pH to 6.0-6.5 "carbopol" 940 resin/0.5 perfume and color/q.s. "laneto" 50/2.0 methyl paraben/0.1 PVP K-30/1.0 gel ethyl plcohol (95%)/7.0
配制方法:
disperse the "carbopol" 940 resin in half of the water with rapid agitation. dissolve the PVP K-30 in the rest of the water. combine the glycerin, "laneto" 50, methyl paraben, and alcohol. add this to the PVP K-30 and water blend. add the triethanolamine in small increments with rapid agitation until a gel forms. add perfume and color.