dissolve the "tergitol" surfactant 15-S-12 and preservative in the water. add the "polymer JR" while stirring, and continue mixing until the resin is dissolved. introduce the alcohol into the formula. finally, add perfume as desired. the use of hot water (≈ 60 C) will increase the rate of solution for "polymer JR."