combine solution of "carbopol" resin and water, dessolve the preservatives in the TEA and glycols and add to the water phase. heat the oil phase to 75 C and add to the water phase at same temperature with mechanical agitation. when emulsion is uniform, cool to 50 C and add the perfume. correct for the evaporated water and continue cooling to room temperature. NOTE: for increased body, "polywax" in place of PEG 400 monostearate results in a soft cream suitable suitable for tube filling.