mink oil/3.5 water/61.5 "promulgen" G/3.0 C) triethanolamine/0.5 B) "lanogene"/5.0 A) "carbopol" 941 resin/0.5 ethanol, SDA 40 (95%)/26.0
配制方法:
add part B to part A at 75 C. cool with continued high speed agitation to 45 C and add part C at room temperature. as part C is added, the batch first thickens considerably, then thins again. NOTE: this base formulation can easily be pigmented if desired. if so, add pigments, premicronized mixture of talc, titanium dioxide and ochre to part B before combining part B with part A in the manufacturing procedure above.