C) aluminum chlorhydroxide (50% aq. sol'n.)/40.00 "extan"-ST/5.00 perfume/q.s. beeswax/2.00 "laxan"-ESS/5.00 B) water/35.00 mineral oil/1.00 A) stearic acid (triple-pressed)/14.00 preservative/--
配制方法:
heat part A to 85 C, part B to 85 C. add part B to part A while stirring. mix while cooling to 40 C. add part C and continue mixing until cool.