mix polybutene with emulsifier in a high-speed, shear mixer such as a cowles dissolver. add water slowly until intersion occurs. add remaining water nore rapidly. preheating both the polymer mixture and the water facilitates emulsification. with the higher viscosity polymers (> 175 cs @ 99 C), temperatures of 65-90 C may be necessary.