配方类型:
POLISHES
配方说明:
配方组成:
dye and perfume/1 g
stoddard solvent or kerosene/3/4 gal
water/to fill drum
"waxenol" 801/1/2 gal
"norfox" IM-38/2 1/2 gal
配制方法:
preblend the "norfox" IM-38 and solvent/kerosene. warm the "waxenol" 801 to 120 F and add to the IM-38-solvent blend. if perfume is used, add it to the preblended ingredients at this point. add water-soluble dye to a small portion of the water and predissolbe.
slowly add warmed (120 F) water to the preblended ingredints.
directions for use: use at a dilution ratio of 140-200:1 for hot wax applications or 110-160:1 for cold or tepid systems. the dye should color the product sufficiently to provede visual identification at the feeding apparatus.