"proto-lan" 4/1.00 triethanolamine/5.00 C) sodium laureth-4 sulfate/5.00 A) methyl paraben/0.10 glycerin/8.00 "supro-tein" V/2.00 B) butyl paraben/0.02 D) "dow corning" 556 fluid/0.20 frahrance/0.50 stearic acid (triple-pressed)/9.00 water/67.68 aerosol coconut acid/1.50
配制方法: