perfume/0.3 kg strontium hydroxide.8H2O/8.9 kg calcium thioglycolate/20.00 kg sodium lauryl sulfate powder/1.5 kg "cellosize" QP 100M/1.0 kg calcium hydroxide/23.1 kg powdered magnesium carbonate (USP)/45.2 kg
配制方法:
1) mix calcium thioglycolate, calcium hydroxide, strontium hydroxide, sodium lauryl sulfate, and "cellosize". 2) blend perfume thoroughly with magnesium carbonate. 3) add #2 to #1 and blend thoroughly. 4) pack in foil or plastic-foil laminated envelopes, each containing 55 g. directions for use: pour contents of one envelope (55 g) into a glass,plastic, or ceramic bowl. avoid metal! add 90 cc of water (3 oz U.S. liquid), and mix thoroughly with a wooden or plastic spoon. do not use a metal spoon!