1) dissolve "copolymer" 937 in water and heat to 45 C. 2) dissolve "emulphor" ON-870 surfactant in ethanol and heat to 45 C. 3) add #2 to #1 and agitate until uniform. 4) add fragrance and cool. 5) charge into container and pressurize with "propellant A-46".