"PVP K-90/1.5 B) titanium dioxide/0.5 PEG-150/7.0 carbomer-940/1.0 laneth-5/3.0 methyl paraben/0.2 PPG-12-buteth-16/8.0 propyl paraben/0.1 D) quaternium-15 (10% aq.sol'n.)/2.0 E) perfume/as desired C) deionized water/25.5 triehanolamine/2.0 A) deionized water/44.5 "merquat" 550/5.0
配制方法:
sprinkle carbomer-940 into rapidly agitating water. heat to 70 C and addtriethanolamine. part A is very thick. in a separate vessel, mix part B to uniform dispersion. add part B to part C and heat to 70 C with stirring. add part C to part A and mix under vacuum to 25 C. add part D and part E with agitation. pH-7.3