water phase: stearyl alcohol/2.5 water/45.5 "amerchol" L-500/2.5 "carbopol" 934/0.5 "glucam" E-20/4.0 cetyl alcohol/2.5 triethanolamine (10% sol'n.)/5.0 perfume and preservatives/q.s. mineral oil (70 visc)/30.0 "solulan" 16/2.5 oil phase: ceresin/5.0
配制方法:
disperse the "carbopol" resin thoroughly in the water using highspeed mixing. add the water phase at 85 C while mixing. when the emulsion has formed, add the triethanolamine. continue mixing to 45 C. add the perfume. mix and cool to 30 C.