glycerin/5.0 "crodamol" PMP/3.0 "germaben"/1.0 "polawax"/6.0 "elastosol"/10.0 B$E: heat oil phase to 75 C, heat water phase to 75 C. add water phase "super refined orange roughy oil"/3.0 to oil phase with good agitation. cool to 30 C. add "elastosol". mix and fill off. $[BF: water phase: "procetyl"/10 oil phase water/69.0