C) "nytal" 400/18.5 water/38.6 kaolin/1.3 A) "veegum"/1.5 titanium dioxide/3.7 iron oxides/1.5 B) "darvan" No.1/0.3 D) isoprpyl myristate/5.0 sorbitan minooleate/0.5 polysorbate 80/1.5 stearyl alcohol/2.0 "amerchol" L-101/2.0 E) perfume and preservative/q.s. propylene glycol/5.0 sodium carboxymethyl cellulose (low visc.)/0.1 fluid matte water/18.5
配制方法:
dry blend the "veegum" and the CMC. add to the water slowly, agitating continually until smooth. micropulverize part C. add to part B amd mull to a smooth pastr. add the pastr to part A and heat to 60-65 C. heat part D to 70 C, and then add to other components. mix until cool.