disperse pigment in 0.225% castor oil. mix the remaining 1,2,3,4, and 5 and heat to 85-90 C with stiring until the polythylene has completely dissolved. add pigment mixture to it. mix slowly, add perfume at 50-55 C and deaerate. pour into mo.ds or containers and allow to cool to room temperature.