帮助中心
配方类型:
ELEMENTARY PREPARATIONS
配方说明:
Glassine Paper
配方组成:
Paper id coated with or dipped in the following solution and then
hung up to dry
Alcohol/30 fl oz
Castor Oil/1 fl oz
Copal Gum/10 oz
配制方法:
Dissolve by letting stand overnight in a covered jar and stirring the next day.