SD-40 Alcohol/45.0 Water/6.8 Disperse the "Laponite" in the water under high shear and then heat to 75'C. Mix Part B and heat to 75'C. Add to Part A under high shear and mix for 30 min. Add Part C and allow to cool while mixing. This product is suitable for aerosol application or, with an increased "Laponite" level, as a gel. Formula No.2 (Gel Stearic Acid/3.0 Deionized Water/66.9 "Arlacel" 60/3.0 "Tween" 60/1.0 "Carbopol" 940/0.5 B: Metadelphene/25.0 Metadelphene/45.0 A: "Laponite" B/1.0 C: Preservative/0.1 "Ethomeen" C/25/2.7
配制方法:
Disperse the "Carbopol" resin in the metadelphene. Add the "Ethomeen" C/25. Add the alcohol-water mixture with mild agitation.