Melt the polyethylene in the oleic acid. Heat to 212-230'C* and add morpholine slowly with stirring. Hold temperature at 208-210'F, add water (heated to 100'C.) slowly with rapid agitation. cover and stir until 104-122'F. Add water to make up to 184. *Avoid open flame.