配方类型:
PAPER
配方说明:
High Wet-Strength Paper Sizing (U.S. Patent 2,549,177)
配方组成:
Oxidized or Chlorinated Starch/1200
Heat for 10 minutes at 80 to 85'F. and add
Glyoxal/24-60
Water/4800
配制方法:
Heat for 5 minutes, dilute to 12 liters with water, and cool. Apply at 110 to 150'F.