METALS AND THEIR TREATMENT
配方说明:
Improved Soldering Flux (U.S. Patent 2,827,408)
配方组成:
Perchloroethylene/30
Lead Chloride/25
Stannous Chloride/50
Silicone Oil (400 centistokes)/2
Ammonium Chloride/8
Cadmium Chloride/20
配制方法:
Use at 675'C. This has an improved shelf life and volatilizes at 600'C. without residue.