The following formulation requires the use of a colloid mill to produce stable emulsion Water/67.9 ARMAK 1714 Paraffin wax/30.00 ARMAK 1574/0.2 Acetic acid/0.4 ARMAK 1959/1.5
配制方法:
The Armak chemicals and paraffin are heated until clear, 140'F. The melt is added in a thin stream to the water-acetic acid mixture also heated to 140'F using good agitation.